Standard UV OPV
formulation contains epoxy oligomer at 30% addition rate.
For greater detail, please click here.
-
Control took 3:00+
minutes til complete foam dispersion vs.
1:49 minutes for formulation containing RadAdd 1116 and FoamZap
UV
-
Foam Generation
Procedure:
1) Mechanical Mixing at 175 rpm for 15 sec. prior to
pouring; and
2) Air introduced via diaphragm pump at a rate of 30 gph
for 30 sec.